The development of today's society is inseparable from nylon products, but the raw materials of nylon products are very tight. Therefore, we must make good use of existing nylon products as much as possible. For example, nylon conveyor belts should be stored in inventory to avoid sun and rain. The nylon conveyor belts that are being produced must also be subject to strict requirements and correct operations to prevent scorching during the use of the conveyor belts, causing certain hazards and waste. Why does the conveyor belt produce scorch? Today, we will analyze the 3 reasons why the nylon conveyor belt produces scorch.
1. Excessive amount of compounding agent in the vulcanization system and too many times of refining will cause scorching.
2. The temperature of the rubber compound is too high and the time is too long; or it is caused by insufficient cooling of the rubber compound.
3. The capacity of the mixed dressing rubber is too large, the temperature is too high, the vulcanizing agent is added too early or the mixing time is too long, it may also cause the conveyor belt to scorch.